Creep Tester mechanical
Multi-station testing system for creep measurement with weight sets
Properties
- Cost-effective multi station systems possible
- Test Load up to 500 N
- Movable Camera System (optional)
Description
The measurement of creep behavior provides data for design purposes as well as for research and development. The test is performed on standardized test specimens under specified conditions, such as pretreatment, temperature and humidity. DIN EN ISO 899 or ASTM D 2990 describe the creep test on plastics for the tensile test and the flexure test. Dead load / lever systems are characterized by simplicity and are suitable for true long-term measurements. With a movable camera system, cost-effective multi-station systems can be created.
![](/fileadmin/_processed_/e/4/csm_10_817_03_24580013ae.jpg)
![](/fileadmin/_processed_/6/5/csm_10_817_01_c4be2bd038.jpg)
Maximum Test Load
500 N / 5 kN
Load Application
Dead Load/ Lever 10:1
Travel
100 mm
Travel Measurement Resolution
optional
Force Measurment Resolution
optional
Temperature Control
optional
Temperature Consistency
optional
Dimensions (D x W x H)
800 x 1040-1820 mm x 2100 mm
Weight
depending on configuration
Mains
depending on configuration
DIN EN ISO 899-1
DIN EN ISO 899-2
ASTM D2990
More products
PIT 25/50 - Pendulum Impact Tester
Impact pendulum for Charpy, Izod and impact tensile tests up to 25/ 50 Joule
IIT 2000 - Instrumented Impact Tester
Puncture and impact resistance measurement up to 2000 Joule
CNC Specimen Milling and Notch Cutter
Fully automated three-axis-machine for test specimen production and processing-bearbeitung